Chemical composition: Blend of various sulfides of alkylphenols
Representative Structural Formula:

Specifications:
| Appearance: |
A deep brown thick material |
Combined Sulfur Content (Total Sulfur Content-Free sulfur Content),%, |
8 |
Free sulfur Content ,%, |
2 |
Kinematic Viscosity (NDF-1 viscometer)(35 )(Pa.S) |
2-15 |
Use:In desulfuration of reclaimed rubber by oil or water oil process, adding 0.3-0.5% of this activator may decrease devulcanization time by 3-6 times and increase product plasticity effectively. Likewise, it is more active for reclaimed SBR and natural rubber, effective apparently for reclaimed neoprene and NBR too.
Packing:Iron drum 200kg.
Standard:Q/ICKZ 02-199